Cited 1 time in
Annealing effects of morphology and luminescence properties of pulsed laser-deposited SrAl2O4: Eu, Dy thin films on sapphire (0001) surfaces
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | Zhang, Zhi-Jun | - |
| dc.contributor.author | Kim, Seunghwan | - |
| dc.contributor.author | Park, Youngsin | - |
| dc.contributor.author | Yang, Woochul | - |
| dc.date.accessioned | 2024-09-26T15:00:58Z | - |
| dc.date.available | 2024-09-26T15:00:58Z | - |
| dc.date.issued | 2017-11 | - |
| dc.identifier.issn | 0040-6090 | - |
| dc.identifier.uri | https://scholarworks.dongguk.edu/handle/sw.dongguk/25556 | - |
| dc.description.abstract | The current work reports on the effect of annealing temperatures on the morphology and photoluminescence properties of SrAl2O4: Eu, Dy thin films on sapphire (0001) substrates fabricated by pulsed laser deposition technique. Scanning electronic microscopy and atomic force microscopy were used to investigate the thickness, surface topography, and the morphology of the films. The film deposited using a higher annealing temperature was packed with a uniform layer of larger particle size grains. In addition, the surface of this film was shown to be relatively rougher than that without annealing treatment. An intense green emission, which is attributed to the 5d-4/transition of Eu2+ was observed at about 520 nm from the films with annealing treatment. The effects of annealing treatment on the morphology, topography, and photoluminescence properties are discussed in detail. | - |
| dc.format.extent | 5 | - |
| dc.language | 영어 | - |
| dc.language.iso | ENG | - |
| dc.publisher | ELSEVIER SCIENCE SA | - |
| dc.title | Annealing effects of morphology and luminescence properties of pulsed laser-deposited SrAl2O4: Eu, Dy thin films on sapphire (0001) surfaces | - |
| dc.type | Article | - |
| dc.publisher.location | 스위스 | - |
| dc.identifier.doi | 10.1016/j.tsf.2017.09.042 | - |
| dc.identifier.scopusid | 2-s2.0-85030549492 | - |
| dc.identifier.wosid | 000413807200042 | - |
| dc.identifier.bibliographicCitation | THIN SOLID FILMS, v.642, pp 290 - 294 | - |
| dc.citation.title | THIN SOLID FILMS | - |
| dc.citation.volume | 642 | - |
| dc.citation.startPage | 290 | - |
| dc.citation.endPage | 294 | - |
| dc.type.docType | Article | - |
| dc.description.isOpenAccess | N | - |
| dc.description.journalRegisteredClass | sci | - |
| dc.description.journalRegisteredClass | scie | - |
| dc.description.journalRegisteredClass | scopus | - |
| dc.relation.journalResearchArea | Materials Science | - |
| dc.relation.journalResearchArea | Physics | - |
| dc.relation.journalWebOfScienceCategory | Materials Science, Multidisciplinary | - |
| dc.relation.journalWebOfScienceCategory | Materials Science, Coatings & Films | - |
| dc.relation.journalWebOfScienceCategory | Physics, Applied | - |
| dc.relation.journalWebOfScienceCategory | Physics, Condensed Matter | - |
| dc.subject.keywordPlus | PHOSPHORS | - |
| dc.subject.keywordPlus | MECHANISM | - |
| dc.subject.keywordPlus | LA | - |
| dc.subject.keywordAuthor | Strontium aluminate | - |
| dc.subject.keywordAuthor | Thin films | - |
| dc.subject.keywordAuthor | Pulsed laser deposition | - |
| dc.subject.keywordAuthor | Luminescence | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
30, Pildong-ro 1-gil, Jung-gu, Seoul, 04620, Republic of Korea+82-2-2260-3114
Copyright(c) 2023 DONGGUK UNIVERSITY. ALL RIGHTS RESERVED.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.