Detailed Information

Cited 0 time in webofscience Cited 27 time in scopus
Metadata Downloads

Structures of delithiated and degraded LiFeBO3, and their distinct changes upon electrochemical cycling

Authors
Bo, S.-H.Nam, K.-W.Borkiewicz, O.J.Hu, Y.-Y.Yang, X.-Q.Chupas, P.J.Chapman, K.W.Wu, L.Zhang, L.Wang, F.Grey, C.P.Khalifah, P.G.
Issue Date
7-Jul-2014
Publisher
American Chemical Society
Citation
Inorganic Chemistry, v.53, no.13, pp 6585 - 6595
Pages
11
Indexed
SCI
SCIE
SCOPUS
Journal Title
Inorganic Chemistry
Volume
53
Number
13
Start Page
6585
End Page
6595
URI
https://scholarworks.dongguk.edu/handle/sw.dongguk/25082
DOI
10.1021/ic500169g
ISSN
0020-1669
1520-510X
Abstract
Lithium iron borate (LiFeBO3) has a high theoretical specific capacity (220 mAh/g), which is competitive with leading cathode candidates for next-generation lithium-ion batteries. However, a major factor making it difficult to fully access this capacity is a competing oxidative process that leads to degradation of the LiFeBO3 structure. The pristine, delithiated, and degraded phases of LiFeBO3 share a common framework with a cell volume that varies by less than 2%, making it difficult to resolve the nature of the delithiation and degradation mechanisms by conventional X-ray powder diffraction studies. A comprehensive study of the structural evolution of LiFeBO3 during (de)lithiation and degradation was therefore carried out using a wide array of bulk and local structural characterization techniques, both in situ and ex situ, with complementary electrochemical studies. Delithiation of LiFeBO3 starts with the production of Li tFeBO3 (t ≈ 0.5) through a two-phase reaction, and the subsequent delithiation of this phase to form Lit-xFeBO3 (x < 0.5). However, the large overpotential needed to drive the initial two-phase delithiation reaction results in the simultaneous observation of further delithiated solid-solution products of Lit-xFeBO3 under normal conditions of electrochemical cycling. The degradation of LiFeBO3 also results in oxidation to produce a Li-deficient phase D-LidFeBO3 (d ≈ 0.5, based on the observed Fe valence of ∼2.5+). However, it is shown through synchrotron X-ray diffraction, neutron diffraction, and high-resolution transmission electron microscopy studies that the degradation process results in an irreversible disordering of Fe onto the Li site, resulting in the formation of a distinct degraded phase, which cannot be electrochemically converted back to LiFeBO3 at room temperature. The Li-containing degraded phase cannot be fully delithiated, but it can reversibly cycle Li (D-Lid+yFeBO3) at a thermodynamic potential of ∼1.8 V that is substantially reduced relative to the pristine phase (∼2.8 V). © 2014 American Chemical Society.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Engineering > Department of Energy and Materials Engineering > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Nam, Kyung Wan photo

Nam, Kyung Wan
College of Engineering (Department of Energy and Materials Engineering)
Read more

Altmetrics

Total Views & Downloads

BROWSE